2mil Polyimide Tape Sheets [10-Packs]

Hover over image to zoom

  • Image 1
  • Image 2
$18.00

 Product Description

2mil Polyimide (Kapton) Tape + Release Liner [10-Packs]

Please contact us if you don't see the size you need.  

3DXTech Polyimide Tape (e.g., Kapton) offers an excellent print surface and is large enough to cover most commercial 3D Printer Platforms.  The polyimide tape is 2mil thick (0.05mm) with Silicone Adhesive and a PET release liner.   This tape provides a smooth heat-resistant surface that easily removes once you have finished your print.  Polyimide tape offers excellent electrical insulation, high temperature resistance, and high voltage resistance.  

Suitable for use on Makerbot Replicator, Makergear, Flashforge, Ultimaker, Prinrbot, Reprap, Mendel, Prusa, Up! Printers, Solidoodle as well as any printer that has a heated bed. 

Technical Specifications

  • Polyimide Substrate (mm):  0.05 ± 0.002  (2mil)
  • Silicone Adhesive (mm):  0.02 ± 0.002
  • PET Release Liner (mm):  0.03 ± 0.002
  • Length (cm) Multiple
  • Width (cm) Multiple
  • Adhesion to Steel Plate (N/25mm):  5.0 – 6.0
  • Tensile Strength (N/25mm):  100 – 140
  • Elongation (%):  35 – 70
  • Voltage Breakdown (KV):  5.0
  • Operating Temperature Range (°C):  -73 - 250

 Product Reviews

  1. Best bed prep for ABS and ASA

    Posted by Mitch on 28th Aug 2016

    This stuff is fantastic for ABS and ASA. The large sheets are a huge improvement over using several smaller strips off of a roll. Not only is the single sheet easier to apply, it will make your bottom layer look much better. If you're careful in your application of the sheet and when you remove prints, you can get a lot of life out of these sheets!


You Recently Viewed...

 

Quick Links

What's News

newsletter

Follow us on

Copyright 2017 3DXTech. All Rights Reserved.
 Sitemap

Click the button below to add the 2mil Polyimide Tape Sheets [10-Packs] to your wish list.