ECOMAX® PLA Biopolymer is made in the USA using 100% virgin PLA biopolymer resin and premium colorants.  Our filament is precision extruded onto 1kg reels (2.2 lbs) and then vacuum-sealed with desiccant to protect it from moisture.  

This filament is ideal for use with practically all desktop printers, such as Makerbot, Reprap, Printrbot jr., Makerfarm Prusa i3, MendelMax, UP! 3D, Flashforge, Solidoodle,
Afinia, Lulzbot Taz, Makergear, Ultimaker, or any other printer accepting 1.75mm or 3.0mm filament.  

Filament diameter specs:  

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  190-220°C, Ideal 200°C
  • Bed Temp:  23-60°C [No Heated Bed Required]
  • Bed Prep:  3DXTech Blue Painters Tape, Hairspray, PVA Glue

 Product Reviews

  1. Consistent and Matte

    Posted by Thanh N. on 5th Dec 2016

    Ecomax Dark Blue PLA prints well at a higher temperature range of 210C or above, and despite the advertised print temperature range of 190C - 220C, I've found that it has a tendency to jam the original all-metal UBIS 13 (no PEEK, no PTFE) at around 190C +- 3C.

    Overall, the filament is very consistent and lends to a consistent extrusion, making for great prints. Unlike a lot of other PLAs from other manufacturers, Ecomax Dark Blue tends to be very matte within this high temperature range, and looks great for fixtures and fasteners, as well as models and robot components.


You Recently Viewed...

 

Quick Links

What's News

newsletter

Follow us on

Copyright 2017 3DXTech. All Rights Reserved.
 Sitemap

Click the button below to add the ECOMAX® Dark Blue PLA Filament to your wish list.