Thermax™ GT High-Temp Bio-Copolyester

Hover over image to zoom

  • Thermax™ GT High-Temp Bio-Copolyester
$34.95

 Product Description

Thermax™ GT High-Temp Bio-Copolyester 

THERMAX™ GT High Temperature Bio-PETG (polyethylene terephthalate glycol copolymer) is a high- temperature resistant bio-copolyester that offers an exceptionally high Tg (110°C), superior chemical resistance, and improved mechanical properties. THERMAX™ GT is BPA-free, dishwasher safe, and made using 12% biomass derived monomer.  

This filament offers higher thermal properties and chemical resistance than ABS - the bio-polymer social responsibility twist of PLA - and the low-warp excellent layer bonding you expect from PETG.  The best of all worlds wrapped up into one amazing filament.  

Diameter Specifications:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm  

Recommended Print Conditions:

  • Extruder Temp:  245 - 270°C
  • Bed Temp: 80-100°C
  • Bed Prep:  Hairspray or Glue Stick on Clean Glass or Build Plate

 Product Reviews

You Recently Viewed...

 

Quick Links

What's News

newsletter

Follow us on

Copyright 2017 3DXTech. All Rights Reserved.
 Sitemap

Click the button below to add the Thermax™ GT High-Temp Bio-Copolyester to your wish list.