Ultra Blue 3DXMAX® ASA (Acrylonitirle Styrene Acrylate) is a UV-resistant weatherable polymer.   Our ASA has a low-gloss matte finish that makes it a perfect filament for technical prints - especially when you don't want the high-gloss surface finish often associated with many other 3D printing materials such as ABS, PETG, or PLA.  ASA's UV-stability makes it an ideal material for outdoor applications that will experience intense exposure to the sun and weather.  ASA's exceptional mechanical and thermal properties - coupled with excellent UV-stability - is why this resin is used the Auto, Marine, and RV industries for exterior applications such as mirror housings, cowl covers, radiator grills, and sensor housings. 

Diameter Specifications:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  235 - 255°C
  • Bed Temp:  90-110°C, cool the bed down by about 10-20°C after the first couple of layers
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry, or Hairspray on clean glass
  • Enclosure:   We recommend using a printer with an enclosure to help keep some heat in while printing with ASA
  • Support:  Our HIPS support works great to create complex parts.  Our HIPS support can be found HERE.  

 Other Details

Test:
Test

 Product Reviews

  1. Pretty good stuff

    Posted by Ryan on 20th Jan 2017

    Prints well at 245C with bed at 90C on geckotek ABS build plate


You Recently Viewed...

 

Quick Links

What's News

newsletter

Follow us on

Copyright 2017 3DXTech. All Rights Reserved.
 Sitemap

Click the button below to add the Ultra Blue ASA Filament to your wish list.