Ultra Blue ASA Filament

3DXMAX® ASA, Ultra Blue 3D Filament, 750g

$29.95

Ultra Blue 3DXMAX® ASA (Acrylonitirle Styrene Acrylate) is a UV-resistant weatherable polymer.   Our ASA has a low-gloss matte finish that makes it a perfect filament for technical prints - especially when you don't want the high-gloss surface finish often associated with many other 3D printing materials such as ABS, PETG, or PLA.  ASA's UV-stability makes it an ideal material for outdoor applications that will experience intense exposure to the sun and weather.  ASA's exceptional mechanical and thermal properties - coupled with excellent UV-stability - is why this resin is used the Auto, Marine, and RV industries for exterior applications such as mirror housings, cowl covers, radiator grills, and sensor housings.   Great low-cost alternative to Zortrax Z-ASA.

Outdoor / UV-Stable / Low-gloss = Great Looking Technical Parts!

Color:  Pantone 2728 (best match)

Diameter Specifications:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  235 - 255°C
  • Bed Temp:  90-110°C, cool the bed down by about 10-20°C after the first couple of layers
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry, or Hairspray on clean glass
  • Enclosure:   We recommend using a printer with an enclosure to help keep some heat in while printing with ASA
  • Support:  Our HIPS support works great to create complex parts.  Our HIPS support can be found HERE.