HIPS 3D Printing Filament

3DXMAX® HIPS, 3D Filament, 1 kg

$29.95 $19.95
(You save $10.00)

3DXMAX® Low-Gloss HIPS 3D Filament

Our low-gloss HIPS (High Impact Polystyrene) 3D printing filament is very easy to print with and allows you to print technical looking parts with a low-gloss matte finish.  HIPS is in the same resin family as ABS and ASA, but is more flexible and has higher impact resistance.  HIPS has good chemical resistance, thermal resistance, and mechanical properties - making it an ideal material for prototype and low-volume production parts.  HIPS does not require drying before processing and can be left on the printer for longer times without moisture issues.  Great low-cost alternative to Zotrax Z-HIPS.  

Benefits of 3DXMAX® Low-Gloss HIPS

  • Low-gloss matte surface finsih
  • Hides layer lines exceptionally well
  • Very low moisture absorption
  • Light weight / low density, 1.04g/cc
  • Excellent ductility and impact resistance
  • Paintable surface

Filament diameter specs:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder:  235- 245°C
  • Bed Temp:  90-110°C
  • Bed Prep:  Kapton Tape, Clean Glass + ABS/Acetone Slurry (ABS Juice)