3DXMAX® PC/ABS 3D Printing Filament

3DXMAX® PC/ABS (polycarbonate + acrylonitrile butadiene styrene) is a premium high-heat 3D printing filament.  PC/ABS alloys the mechanical properties & high-heat resistance of PC with the printability of ABS and allows for the printing of functional prototypes and production parts with very fine detail and excellent surface quality.  3DXMAX® Low-Gloss PC/ABS is suitable for use in both consumer-grade and industrial FDM/FFF printers that have a heated print bed.   Made by 3DXTECH® in the USA.

Filament Diameter Specs:  

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  270-290°C
  • Bed Temp:  110 - 120°C
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry
  • Enclosure:   Although not 100% necessary, we recommend using a printer with an enclosure to help keep some heat in while printing with PC/ABS
  • Support:  Our Aquatek water soluble support works great to create complex parts.  This support can be found HERE.  
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.