5-Pack ABS 3D Printing Filament

3DXTECH™ ABS, 4kg Reels, 5-Pack Special Order

$495.00
Lead-time:
2 to 3 Weeks

4KG XL Reels of ABS 3D Printing Filament 5-Pack [Special Order]

3DXTech™ ABS is made in the USA using 100% virgin resin and colorants - precision extruded onto 4kg reels (8.8 lbs.).  The filament is then vacuum-sealed with desiccant to protect it from moisture.  For use with practically ANY desktop printer that can print with ABS (heated print bed) - including Airwolf, Ultimaker, Makerbot, Reprap, Printrbot jr., Makerfarm Prusa i3, MendelMax, UP! 3D, Flashforge, Solidoodle, Afinia, Lulzbot Taz (all models), Makergear...\

Please note:

  • This product is made to order, please allow up to 2 to 3 weeks lead time for your order to be produced and ready to ship
  • All other products in your order will ship with the 5-pack (no partial shipments)
  • One color only in 5-packs (no mixing of colors)

Reel Specs:

  • 12" diameter, 4" traverse, 2" arbor hole

Filament diameter specs:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  220-240°C, Ideal 230°C
  • Bed Temp:  100-110°C
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry