ABS - 4kg Reel

3DXTECH® ABS, 4kg

$99.95

4KG XL Reels of ABS 3D Printing Filament

3DXTech™ ABS is made in the USA using 100% virgin resin and colorants - precision extruded onto 4kg reels (8.8 lbs.).  The filament is then vacuum-sealed with desiccant to protect it from moisture.  

Print industrial-grade ABS parts with Gearbox™ HT2 High-Temp 3D Printer.  Check it out HERE. 

For use with practically ANY desktop printer that can print with ABS (heated print bed), including Airwolf, Ultimaker, Makerbot, Reprap, Prusa i3, MendelMax, UP! 3D, Flashforge, Solidoodle, Afinia, Lulzbot Taz (all models), Makergear...

 
Reel Specs:
  • 12" diameter, 4" traverse, 2" arbor hole

Filament diameter specs:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  220-240°C, Ideal 230°C
  • Bed Temp:  100-110°C
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry
  • Support Material:  We recommend our AquaTek™ water soluble support - HERE
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.