ABS 3D Printing Filament, 1kg Reel
3DXTech™ ABS is made in the USA using 100% virgin resin and colorants - precision extruded onto 1kg reels (2.2 lbs.). The filament is then vacuum-sealed with desiccant to protect it from moisture.
Print industrial-grade ABS parts with Gearbox™ HT2 High-Temp 3D Printer. Check it out HERE.
Filament diameter specs:
- 1.75mm +/- 0.05mm
- 2.85mm +/- 0.05mm
Recommended Print Conditions: