Transparent ABS 3D Printing Filament

ABScent™ ABS, 3D Filament, 750g [SALE] [Discontinued]

$29.95 $14.95
(You save $15.00)

ABScent® Transparent ABS.  

ABScent™ ABS is transparent and odorless premium 3D printing filament formulated utilizing high-flow MABS [methylmethacrylate acrylonitrile butadiene styrene] resin and colorants. ABScent™ ABS offers superior mechanical properties to most ABS filaments, absent the odor. MABS is an amorphous acrylic-modified ABS polymer that has practically no odor – especially when compared to traditional ABS resins. This makes it ideal for printing in public spaces, schools, and office environments. 

Diameter Specifications:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

1-3d-filament-technical-data.png

Recommended Print Conditions:

  • Extruder Temp:  230 - 260°C.  In-house testing indicates best toughness and clarity above 250°C.   
  • Extruder Speed:  4000mm/min
  • Bed Temp:  90-110°C
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry
  • Support:  Our HIPS support works great to create complex parts.  Our HIPS support can be found HERE.