Zortrax – UP – Afinia A2 Hardened Steel Nozzle
The Zortrax – UP – Afinia A2 Hardened Steel Nozzle is manufactured in the USA by Performance 3D using heat treated A2 tool steel and coated with Duraplat3-d™ wear-resistant coating for enhanced wear and flow. Compared to stainless steel nozzles, Hercules™ nozzles are 3X harder, have 50% better heat transfer, and 5x the wear life. Hercules™ nozzles are the clear cut choice for printing with more abrasive filaments like our CarbonX™ Carbon Fiber grades.
Wear resistant high lubricity nozzles compatible with the popular Afinia / Up hotend extruders.
Compatibility
- Zortrax M200
- Zortrax M300
- Afinia H479
- Afinia H480-01
- UP Plus
- UP Plus 2
- UP mini
Features
- 0.4mm orifice
- M6 thread
- 1.75mm filament
- Use with existing 3.5mm printer insert