AmideX™ Nylon 6 Copolymer

AmideX™ Nylon 6/66 Copolymer

$38.00

AmideX™ Nylon 6/66 Copolymer

AmideX™ Nylon 6/66 copolymer has been formulated for superior printability and high-performance.  Nylon is the go-to engineering-grade of thermoplastic in the world based on its excellent mechanical, thermal, and chemical resistance properties.   We manufacture AmideX™ Nylon filament at our factory in Grand Rapids MI using prime resin and state-of-the-art extrusion equipment.  

Product Attributes

  • Excellent printability
  • High Strength:  60 MPa / 8700 PSI Tensile Strength
  • Improved chemical resistance vs traditional materials in 3D
  • Abrasion / wear resistance
  • Thermal properties:  Tg = 85°C, Tm = 200°C

Chemical Resistance Chart

Nylon chemical resistance chart

Filament Diameter Specs

  • 1.75mm, +/- 0.05mm
  • 2.85mm, +/- 0.05mm

Recommended Print Conditions

  • Extruder: 255-275°C
  • Bed Temp: 60-70°C
  • Bed Prep: Polyimide (Kapton), PEI (ULTEM™) Sheet, Garolite, BuildTak
  • Chamber / Ambient Temp:  Not required, but using a 30-80°C printer chamber allows for superior layer bonding & mechanical properties.
  • Support:  Our Aquatek water soluble support works great to create complex parts.  This support can be found HERE.  
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.