AquaTek™ PVA Water Soluble Support Filament, 750g

$90.00

AquaTek™ PVA Support Filament

Our PVA is an advanced water-soluble support filament for printing complex parts.  PVA (Poly Vinyl Alcohol Co-polymer) is water-soluble and is easily removed from the printed part with room-temp water.   Extruded by 3DXTECH using state-of-the-art equipment at our plant in Grand Rapids, MI.  

Note:  Keep PVA dry and store filament in the zip-lock mylar that is supplied with desiccant or in a sealed container with desiccant.  

AquaTek™ PVA Attributes:

  • PVA is readily soluble in water
  • Ideal support material printing complex geometry parts

Filament diameter specs:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder:  190-220°C
  • Bed Temp:  60-90°C