Carbon Fiber ABS for Fortus® 360/400/900mc Printers

Carbon Fiber ABS Refill for Fortus® 360/400/900mc Printers (92in3)

$395.00 $275.00
(You save $120.00)

TriMax™ Carbon Fiber ABS

100% compatible with Stratasys® Fortus® 360/400/900mc printers using the M30 ABS EEPROM Chip (provided in the order).  

TriMax™ CF-ABS is a high-performance carbon fiber reinforced ABS filament ideal for anyone that desires a structural component with high modulus, excellent surface quality, dimensional stability, light weight, and ease of printing.  Made using Sabic® MG-94 premium ABS and High-Modulus Carbon Fiber.

Please note:  We performed hundreds of hours of testing on this grade in Fortus® printers - both on our in-house printers and with outside beta testers.  Due to the abrasive nature of carbon fiber, you should anticipate a 50% reduction in tip-life due to higher wear rates vs. unfilled ABS.

View Data Sheets Here.