{"title":"End-Use Parts - Extreme Performance \u0026 Aerospace","description":"\u003cp data-start=\"4771\" data-end=\"4921\"\u003eThese advanced materials deliver exceptional thermal, chemical, and mechanical resistance for aerospace, defense, and extreme industrial applications.\u003c\/p\u003e\n\u003cp data-start=\"4923\" data-end=\"5079\"\u003e\u003cstrong data-start=\"4923\" data-end=\"4936\"\u003eBest For:\u003c\/strong\u003e\u003cbr data-start=\"4936\" data-end=\"4939\"\u003e• Aerospace-grade components\u003cbr data-start=\"4967\" data-end=\"4970\"\u003e• Chemical and thermal extremes\u003cbr data-start=\"5001\" data-end=\"5004\"\u003e• High-performance production parts\u003cbr data-start=\"5039\" data-end=\"5042\"\u003e• Advanced engineering applications\u003c\/p\u003e\n\u003cp data-start=\"5081\" data-end=\"5161\"\u003e\u003cstrong\u003e\u003cem data-start=\"5081\" data-end=\"5161\"\u003e*Requires high-temperature capable printers and advanced processing conditions.*\u003c\/em\u003e\u003c\/strong\u003e\u003c\/p\u003e","products":[{"product_id":"carbonx-peek-cf10-1","title":"CarbonX PEEK+CF10","description":"\u003cdiv class=\"pdp-description-row\"\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\n\u003ch2\u003eCarbonX PEEK+CF10\u003c\/h2\u003e\n\u003cp\u003eCarbonX PEEK+CF10 is one of the premier polymers in FFF\/FDM 3D Printing. Made using 10% high-modulus chopped carbon fiber for exceptional stiffness, strength, and dimensional stability.\u003c\/p\u003e\n\u003cp\u003ePEEK+CF10 is one of the highest performance thermoplastics ever invented. It is used in some of the most demanding applications by industries such as Auto, Aerospace, Defense, Semi-conductor, and Oil\/Gas. Engineers depend on PEEK for applications where failure is not an option.\u003c\/p\u003e\n\u003cp data-end=\"486\" data-start=\"0\"\u003ePEEK is an advanced, ultra-high-temperature polymer that demands industrial printing conditions to achieve consistent results. Plan on a 360–450°C hot end, 120–160°C bed, and a fully enclosed, actively heated chamber (70–150°C) to control warping and ensure strong layer adhesion. Best practices also include thorough filament drying, slow print speeds, and reduced or disabled part-cooling fan. Most standard desktop printers can’t reliably maintain these conditions.\u003c\/p\u003e\n\u003ch4 data-end=\"866\" data-start=\"488\"\u003e\u003cstrong\u003eFor greater success, we recommend these high performance filaments:\u003c\/strong\u003e\u003c\/h4\u003e\n\u003cp data-is-only-node=\"\" data-is-last-node=\"\" data-end=\"866\" data-start=\"488\"\u003e\u003ca href=\"https:\/\/www.3dxtech.com\/collections\/pekk\"\u003e\u003cstrong data-start=\"265\" data-end=\"274\" data-is-only-node=\"\"\u003ePEKK:\u003c\/strong\u003e\u003c\/a\u003e Delivers similar “PEAK-family” performance benefits but is often considered more forgiving to dial in than PEEK, with improved layer bonding and reduced warping sensitivity in many setups. It’s a strong step toward PEEK-level capability without as much process difficulty.\u003c\/p\u003e\n\u003cp data-is-only-node=\"\" data-is-last-node=\"\" data-end=\"866\" data-start=\"488\"\u003e\u003ca href=\"https:\/\/www.3dxtech.com\/collections\/pei-ultem\"\u003e\u003cstrong data-start=\"2\" data-end=\"19\" data-is-only-node=\"\"\u003eULTEM™ (PEI):\u003c\/strong\u003e\u003c\/a\u003e A high-performance polymer that typically prints more predictably than PEEK while still offering excellent heat resistance and strength. It’s a great choice when you want industrial-level performance with a more manageable processing window.\u003c\/p\u003e\n\u003cp data-is-only-node=\"\" data-is-last-node=\"\" data-end=\"866\" data-start=\"488\"\u003e\u003ca href=\"https:\/\/www.3dxtech.com\/products\/thermax-pps\"\u003e\u003cstrong data-start=\"551\" data-end=\"559\" data-is-only-node=\"\"\u003ePPS:\u003c\/strong\u003e\u003c\/a\u003e Known for strong chemical resistance and dimensional stability, and it can be an easier path to consistent parts compared to PEEK. It’s a smart option for environments involving fuels, solvents, or harsh chemicals where reliability matters.\u003c\/p\u003e\n\u003ch5\u003eMADE IN THE USA\u003c\/h5\u003e\n\u003cp\u003eWe manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.\u003c\/p\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\u003cimg src=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/CF-PEEK-Part.png?v=1741639048\"\u003e\u003c\/div\u003e\n\u003c\/div\u003e","brand":"3DXTECH","offers":[{"title":"Black \/ 1.75mm \/ 250g","offer_id":43809000620085,"sku":"PK003CF200250BK00","price":195.0,"currency_code":"USD","in_stock":true},{"title":"Black \/ 1.75mm \/ 500g","offer_id":43867413938229,"sku":"PK003CF200500BK00","price":400.0,"currency_code":"USD","in_stock":true},{"title":"Black \/ 1.75mm \/ 1kg","offer_id":43779587375157,"sku":"PK003CF201000BK00","price":715.0,"currency_code":"USD","in_stock":true},{"title":"Black \/ 1.75mm \/ 2kg","offer_id":43809000685621,"sku":"PK003CF202000BK00","price":1195.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/215-CF10-PEEK-175mm-Black-500g-3D-Printer-Filament.png?v=1722621158"},{"product_id":"carbonx-pekk-a-cf15-1","title":"CARBONX PEKK-A+CF15","description":"\u003cdiv class=\"pdp-description-row\"\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\n\u003ch2\u003eCARBONX PEKK-A+CF15\u003c\/h2\u003e\n\u003cp\u003eCarbonX™ Carbon Fiber PEKK-A (PolyEtherKetoneKetone) 3D filament is made using PEKK (60\/40 copolymer) and 15% high modulus chopped carbon fiber.  A leading material in the PAEK family, PEKK has exceptionally good mechanical, thermal, and chemical resistance properties while offering ease of printing.\u003c\/p\u003e\n\u003ch5\u003eMADE IN THE USA\u003c\/h5\u003e\n\u003cp\u003eWe manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.\u003c\/p\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\u003cimg src=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/Black_Conveyor_Housing_2.png?v=1741695165\"\u003e\u003c\/div\u003e\n\u003c\/div\u003e","brand":"3DXTECH","offers":[{"title":"Black \/ 1.75mm \/ 250g","offer_id":43866670006325,"sku":"PKK08CF200250BK00","price":88.0,"currency_code":"USD","in_stock":true},{"title":"Black \/ 1.75mm \/ 750g","offer_id":43841088978997,"sku":"PKK08CF200750BK00","price":250.0,"currency_code":"USD","in_stock":true},{"title":"Black \/ 1.75mm \/ 2kg","offer_id":43779586162741,"sku":"PKK08CF202000BK00","price":665.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/CF15_PEKK-A_175mm_2kg-1_b594870e-45c5-4269-99d5-e441c995bfcf.jpg?v=1722618907"},{"product_id":"thermax-peek-1","title":"ThermaX PEEK","description":"\u003cdiv class=\"pdp-description-row\"\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\n\u003ch2\u003eThermaX PEEK\u003c\/h2\u003e\n\u003cp\u003eThermaX PEEK (PolyEtherEtherKetone) is one of the highest-performance polymers in the world. In fact, it’s one of the highest-performance plastics ever invented. PEEK has exceptional mechanical, thermal, and chemical resistance properties making it a go-to material in some of the most demanding applications where failure is not an option.\u003c\/p\u003e\n\u003cp data-end=\"486\" data-start=\"0\"\u003ePEEK is an advanced, ultra-high-temperature polymer that demands industrial printing conditions to achieve consistent results. Plan on a 360–450°C hot end, 120–160°C bed, and a fully enclosed, actively heated chamber (70–150°C) to control warping and ensure strong layer adhesion. Best practices also include thorough filament drying, slow print speeds, and reduced or disabled part-cooling fan. Most standard desktop printers can’t reliably maintain these conditions.\u003c\/p\u003e\n\u003ch4 data-end=\"866\" data-start=\"488\"\u003e\u003cstrong\u003eFor greater success, we recommend these high performance filaments:\u003c\/strong\u003e\u003c\/h4\u003e\n\u003cp data-is-only-node=\"\" data-is-last-node=\"\" data-end=\"866\" data-start=\"488\"\u003e\u003ca href=\"https:\/\/www.3dxtech.com\/collections\/pekk\"\u003e\u003cstrong data-start=\"265\" data-end=\"274\" data-is-only-node=\"\"\u003ePEKK:\u003c\/strong\u003e\u003c\/a\u003e Delivers similar “PEAK-family” performance benefits but is often considered more forgiving to dial in than PEEK, with improved layer bonding and reduced warping sensitivity in many setups. It’s a strong step toward PEEK-level capability without as much process difficulty.\u003c\/p\u003e\n\u003cp data-is-only-node=\"\" data-is-last-node=\"\" data-end=\"866\" data-start=\"488\"\u003e\u003ca href=\"https:\/\/www.3dxtech.com\/collections\/pei-ultem\"\u003e\u003cstrong data-start=\"2\" data-end=\"19\" data-is-only-node=\"\"\u003eULTEM™ (PEI):\u003c\/strong\u003e\u003c\/a\u003e A high-performance polymer that typically prints more predictably than PEEK while still offering excellent heat resistance and strength. It’s a great choice when you want industrial-level performance with a more manageable processing window.\u003c\/p\u003e\n\u003cp data-is-only-node=\"\" data-is-last-node=\"\" data-end=\"866\" data-start=\"488\"\u003e\u003ca href=\"https:\/\/www.3dxtech.com\/products\/thermax-pps\"\u003e\u003cstrong data-start=\"551\" data-end=\"559\" data-is-only-node=\"\"\u003ePPS:\u003c\/strong\u003e\u003c\/a\u003e Known for strong chemical resistance and dimensional stability, and it can be an easier path to consistent parts compared to PEEK. It’s a smart option for environments involving fuels, solvents, or harsh chemicals where reliability matters.\u003c\/p\u003e\n\u003ch5\u003eMADE IN THE USA\u003c\/h5\u003e\n\u003cp\u003eWe manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.\u003c\/p\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\u003cimg src=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/PEEK_Part_2.png?v=1741638782\"\u003e\u003c\/div\u003e\n\u003c\/div\u003e","brand":"3DXTECH","offers":[{"title":"Natural \/ 1.75mm \/ 250g","offer_id":43809002717237,"sku":"PK001UN200250NAT0","price":158.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 500g","offer_id":43867413282869,"sku":"PK001UN200500NAT0","price":385.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 1kg","offer_id":43779575578677,"sku":"PK001UN201000NAT0","price":588.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 2kg","offer_id":43809002782773,"sku":"PK001UN202000NAT0","price":1175.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/442-PEEK-175mm-Natural-500g-3D-Printer-Filament.png?v=1722621391"},{"product_id":"thermax-pei-1010","title":"ThermaX PEI 1010","description":"\u003cdiv class=\"pdp-description-row\"\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\n\u003ch2\u003eThermaX PEI 1010\u003c\/h2\u003e\n\u003cp\u003e3DXTECH produces this 3D printing filament using a specialty compound custom-formulated using ULTEM 1010 PEI resin. PEI is an amorphous, high-performance polymer that combines excellent mechanical, thermal, and chemical resistance properties.\u003cbr\u003e\u003cbr\u003eOur PEI based filaments offer the ability to create parts with excellent properties at elevated temperatures due to a very high glass transition temperature (Tg). Ideal for use in critical applications which require electrostatic discharge (ESD) protection, a high level of cleanliness, and the outstanding thermal and chemical properties you’ve come to expect with PEI based compounds.\u003c\/p\u003e\n\u003ch5\u003eMADE IN THE USA\u003c\/h5\u003e\n\u003cp\u003eWe manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.\u003c\/p\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\u003cimg src=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/CF_Mold_End.png?v=1741696019\"\u003e\u003c\/div\u003e\n\u003c\/div\u003e","brand":"3DXTECH","offers":[{"title":"Black \/ 1.75mm \/ 250g","offer_id":53019535147371,"sku":"PEI02UN200250BK01","price":70.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 250g","offer_id":43809003012149,"sku":"PEI02UN200250NAT0","price":70.0,"currency_code":"USD","in_stock":true},{"title":"Black \/ 1.75mm \/ 500g","offer_id":53019535180139,"sku":"PEI02UN200500BK01","price":98.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 500g","offer_id":43818700177461,"sku":"PEI02UN200500NAT0","price":98.0,"currency_code":"USD","in_stock":true},{"title":"Black \/ 1.75mm \/ 1kg","offer_id":53019535212907,"sku":"PEI02UN201000BK01","price":195.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 1kg","offer_id":51618342437227,"sku":"PEI02UN201000NAT0","price":195.0,"currency_code":"USD","in_stock":true},{"title":"Black \/ 1.75mm \/ 2kg","offer_id":53019535245675,"sku":"PEI02UN202000BK01","price":390.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 2kg","offer_id":43809003110453,"sku":"PEI02UN202000NAT0","price":390.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/251-Ultem1010-175mm-Natural-500g-3D-Printer-Filament.png?v=1722621400"},{"product_id":"thermax-pei-9085","title":"ThermaX PEI 9085","description":"\u003cdiv class=\"pdp-description-row\"\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\n\u003ch2\u003eThermaX PEI 9085\u003c\/h2\u003e\n\u003cp\u003e3DXTECH produces this 3D printing filament using a specialty compound custom-formulated using ULTEM 9085 resin. ULTEM PEI is an amorphous, high-performance polymer that combines excellent mechanical, thermal, and chemical resistance properties.\u003c\/p\u003e\n\u003cp\u003eOur PEI-based filaments offer the ability to create parts with excellent properties at elevated temperatures due to a very high glass transition temperature (Tg). Ideal for use in critical applications which require electrostatic discharge (ESD) protection, a high level of cleanliness, and the outstanding thermal and chemical properties you’ve come to expect with PEI based compounds.\u003c\/p\u003e\n\u003ch5\u003eMADE IN THE USA\u003c\/h5\u003e\n\u003cp\u003eWe manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.\u003c\/p\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\u003cimg src=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/9085-Part.png?v=1741696283\"\u003e\u003c\/div\u003e\n\u003c\/div\u003e","brand":"3DXTECH","offers":[{"title":"Black \/ 1.75mm \/ 250g","offer_id":53019599503723,"sku":"PEI01UN200250BK01","price":80.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 250g","offer_id":43809004585013,"sku":"PEI01UN200250NAT0","price":80.0,"currency_code":"USD","in_stock":true},{"title":"Black \/ 1.75mm \/ 500g","offer_id":53019599536491,"sku":"PEI01UN200500BK01","price":145.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 500g","offer_id":43818699948085,"sku":"PEI01UN200500NAT0","price":145.0,"currency_code":"USD","in_stock":false},{"title":"Scarlet \/ 1.75mm \/ 500g","offer_id":43818699980853,"sku":"PEI01UN200500RD00","price":130.5,"currency_code":"USD","in_stock":true},{"title":"Black \/ 1.75mm \/ 1kg","offer_id":53019599569259,"sku":"PEI01UN201000BK01","price":220.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 1kg","offer_id":43809004650549,"sku":"PEI01UN201000NAT0","price":220.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 2kg","offer_id":43809004683317,"sku":"PEI01UN202000NAT0","price":440.0,"currency_code":"USD","in_stock":false}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/234-Ultem9085-175mm-Natural-500g-3D-Printer-Filament.png?v=1722619090"},{"product_id":"pekk-a","title":"THERMAX PEKK A","description":"\u003cdiv class=\"pdp-description-row\"\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\n\u003ch2\u003eTHERMAX PEKK A\u003c\/h2\u003e\n\u003cp\u003eThermaX PEKK (PolyEtherKetoneKetone) is made using Arkema Kepstan PEKK and is one of the highest-performance polymers in plastics business. A leading material in the PAEK family, PEKK has exceptionally good mechanical, thermal, and chemical resistance properties. It is also not only substantially easier to print than PEEK, it’s one of the easiest ultra-polymers to 3D print period. Developed in partnership with Arkema, a leading supplier of ultra-performance materials.\u003c\/p\u003e\n\u003ch5\u003eMADE IN THE USA\u003c\/h5\u003e\n\u003cp\u003eWe manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.\u003c\/p\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\u003cimg src=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/PEKK-Part.png?v=1741694881\"\u003e\u003c\/div\u003e\n\u003c\/div\u003e","brand":"3DXTECH","offers":[{"title":"Natural \/ 1.75mm \/ 250g","offer_id":43809007599669,"sku":"PKK04UN200250NAT0","price":175.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 500g","offer_id":43867414134837,"sku":"PKK04UN200500NAT0","price":295.0,"currency_code":"USD","in_stock":true},{"title":"Black \/ 1.75mm \/ 500g","offer_id":53019535442283,"sku":"PKK09UN100500BK01","price":295.0,"currency_code":"USD","in_stock":false},{"title":"Natural \/ 1.75mm \/ 1kg","offer_id":43808131350581,"sku":"PKK04UN201000NAT0","price":550.0,"currency_code":"USD","in_stock":true},{"title":"Black \/ 1.75mm \/ 1kg","offer_id":53019533377899,"sku":"PKK09UN101000BK01","price":550.0,"currency_code":"USD","in_stock":true},{"title":"Natural \/ 1.75mm \/ 2kg","offer_id":43808131383349,"sku":"PKK04UN202000NAT0","price":995.0,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/Black-PEKK.png?v=1722619099"}],"url":"https:\/\/www.3dxtech.com\/collections\/end-use-parts-extreme-performance-aerospace.oembed","provider":"3DXTECH","version":"1.0","type":"link"}