High Temp PLA - Dark Grey

ECOMAX® HT High Temperature PLA, Dark Grey



ECOMAX® High Temperature PLA Biopolymer is made in the USA using 100% virgin High Temp Natureworks High-Temp PLA biopolymer resin and premium colorants.  Our filament is precision extruded onto 1kg reels (2.2 lbs) and then vacuum-sealed with desiccant to protect it from moisture.  

Once you anneal parts made with this material, you can expect a substantial increase your thermal and mechanical properties.  This PLA prints like normal PLA, but offers almost double the thermal properties - up to 120°C (test data coming soon!)

This filament is ideal for use with practically all desktop printers, such as Makerbot, Reprap, Printrbot jr., Makerfarm Prusa i3, MendelMax, UP! 3D, Flashforge, Solidoodle, Afinia, Lulzbot Taz, Makergear, Ultimaker, or any other printer accepting 1.75 or 2.85mm filament.     

Filament diameter specs:  

  • 1.75mm +/- 0.03mm
  • 2.85mm +/- 0.03mm

Recommended Print Conditions:

  • Extruder Temp:  190-220°C, Ideal 200°C
  • Bed Temp:  23-60°C [No Heated Bed Required]
  • Bed Prep:  3DXTech Blue Painters Tape, Hairspray or PVA Glue on clean glass

Annealing Directions:

  • Place the printed part in an oven at 80°C for 30-60minutes.  You may want to leave any supports on the part to help support it if you're concerned about deflection.  The additional heat will further crystallize the PLA and increase the heat distortion temperature (HDT) to upwards of 120°C!