3DXSTAT™ ESD-TPU Elastomer Filament

3DXSTAT™ ESD TPC Flexible 3D Filament

$98.00

3DXSTAT™ ESD-TPC Elastomer Filament, SEMI-FLEX 95A

3DXSTAT™ ESD-Safe TPC [thermoplastic copolyester] elastomer is an engineering-grade thermoplastic chosen for its balance of excellent flexibility, ease of printing, chemical resistance, and toughness.  3DXSTAT™ ESD-TPC elastomeric filament has been formulated to offer ESD-Safe electrical conductivity with a target surface resistance of 10^7 to 10^9 Ohm.  

Semi-Flex Hardness: Shore 95A

Benefits of 3DXSTAT™ ESD-TPC Filament:

  • High elongation (>300%)
  • ESd-Safe:  10^6 - 10^9 Ohm/sq surface resistance
  • Ease of printing
  • Excellent layer bonding
  • Outstanding fatigue resistance
  • Very low odor while printing
  • Low moisture absorption
  • Retains flexibility even at low temperatures
  • Styrene and BPA Free

Filament Diameter Specs:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  245-265°C 
  • Bed Temp:  23-70°C
  • Bed Prep:  Hairspray or Glue Stick on clean glass
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.