Firewire® Flame Retardant ABS 3D Printing Filament, 1kg Reel
Firewire® FR-ABS is made using a premium UL94 V-0 rated ABS. Our FR-ABS is high-gloss jet black and supplied on 1kg reels (2.2 lbs.), sealed in vacuum bags to keep them dry. This filament is ideal for applications that require UL94 V-0 self-extinguishing characteristics.
Print industrial-grade FR-ABS parts with Gearbox™ HT2 High-Temp 3D Printer. Check it out HERE.
Flame Rating (UL94)*
- 1.5mm: V-0
- 2.0mm: V-0, 5VB
- 2.5mm: V-0, 5VB
- 3.0mm: V-0, 5VB
Filament diameter specs:
- 1.75mm +/- 0.05mm
- 2.85mm +/- 0.05mm
Recommended Print Conditions:
- Extruder Temp: 220-240°C, Ideal 230°C
- Bed Temp: 100-110°C
- Bed Prep: 3DXTech Polyimide Tape, ABS / Acetone Slurry
- Support: Our Aquatek water soluble support works great to create complex parts. This support can be found HERE.
- Drying Instructions: Please see the following instructions for when you want to dry out this filament, HERE.
Please note: Direct ventilation from your printer is required to print Firewire® ABS. This grade has a much more pronounced odor during printing and we highly recommend venting outside or via HEPA and carbon filtration.
*This is the UL94 rating of base resin we use to make Firewire® FR-ABS Filament.