HIPS Support Filament

3DXMAX™ HIPS Filament

$24.95

3DXMax™ HIPS Support Material

Manufactured in the USA from 100% virgin HIPS (High Impact Polystyrene) resin.  We use state-of-the-art resins & manufacturing technologies to give you the best possible printing experience.

Precision extruded from our own formulated HIPS.  This grade of HIPS is a bit different than the HIPS used to make our colors and formulated to be more sensitive to attack from d-limonene solvent. 

Filament diameter specs:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder:  220 - 235°C  [printing with higher temps will make a stronger / tougher support, which may be more difficult to remove]
  • Bed Temp:  100-110°C
  • Bed Prep:  Kapton Tape, ABS/Acetone Slurry on clean glass