3DXMAX® ASA (Acrylonitirle Styrene Acrylate) is a UV-resistant weatherable polymer.   Our ASA has a low-gloss matte finish that makes it a perfect filament for technical prints - especially when you don't want the high-gloss surface finish often associated with many other 3D printing materials such as ABS, PETG, or PLA.  ASA's UV-stability makes it an ideal material for outdoor applications that will experience intense exposure to the sun and weather.  ASA's exceptional mechanical and thermal properties - coupled with excellent UV-stability - is why this resin is used the Auto, Marine, and RV industries for exterior applications such as mirror housings, cowl covers, radiator grills, and sensor housings. 

Print industrial-grade ASA parts with Gearbox™ HT2 High-Temp 3D Printer.  Check it out HERE. 

Please note:

  • This product is made to order, please allow a 2 to 3 week lead time for your order to be produced and ready to ship
  • All other products in your order will ship with the 5-pack (no partial shipments)
  • One color only in 5-packs (no mixing of colors)

Diameter Specifications:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Reel Specs:

  • 12" diameter, 4" traverse, 2" arbor hole

Recommended Print Conditions:

  • Extruder Temp:  235 - 255°C
  • Bed Temp:  90-110°C, cool the bed down by about 10-20°C after the first couple of layers
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry, or Hairspray on clean glass
  • Enclosure:   We recommend using a printer with an enclosure to help keep some heat in while printing with ASA
  • Support:  Our Aquatek water soluble support works great to create complex parts.  This support can be found HERE.  
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.