3DXMAX® ASA (Acrylonitirle Styrene Acrylate) is a UV-resistant weatherable polymer. Our ASA has a low-gloss matte finish that makes it a perfect filament for technical prints - especially when you don't want the high-gloss surface finish often associated with many other 3D printing materials such as ABS, PETG, or PLA. ASA's UV-stability makes it an ideal material for outdoor applications that will experience intense exposure to the sun and weather. ASA's exceptional mechanical and thermal properties - coupled with excellent UV-stability - is why this resin is used the Auto, Marine, and RV industries for exterior applications such as mirror housings, cowl covers, radiator grills, and sensor housings. Great low-cost alternative to Zortrax Z-ASA.
Print industrial-grade ASA parts with Gearbox™ HT2 High-Temp 3D Printer. Check it out HERE.
Diameter Specifications:
- 1.75mm +/- 0.05mm
- 2.85mm +/- 0.05mm
Reel Specs:
- 12" diameter, 4" traverse, 2" arbor hole
Recommended Print Conditions:
- Extruder Temp: 235 - 255°C
- Bed Temp: 90-110°C, cool the bed down by about 10-20°C after the first couple of layers
- Bed Prep: 3DXTech Polyimide Tape, ABS / Acetone Slurry, or Hairspray on clean glass
- Enclosure: We recommend using a printer with an enclosure to help keep some heat in while printing with ASA
- Support: Our Aquatek water soluble support works great to create complex parts. This support can be found HERE.
- Drying Instructions: Please see the following instructions for when you want to dry out this filament, HERE.