HIPS Pellets

Ideal for home extrusion enthusiasts.  Make your own high-performance HIPS Support filament with a home-extruder such as the Filabot, Filastruder, and Noztek.  Rapidly dissolves in d-Limonene and makes the perfect support filament. 

Please note:  Additional shipping charges may apply on orders over 10 pounds

Processing Recommendations:

  • Pre-dry before extrusion at 80°C for 2-4 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  190 - 210°C