INTAMSYS Funmat HT

The Funmat HT is a high-performance 3D printer can print a wide array of materials from general-purpose materials like ABS and PLA up to ultra-performance materials including PEEK, PEI and PPSU.  The Funmat HT boasts a 450°C hot-end with a patent-pending heated chamber capable of holding 90°C, and a 160°C heated print bed. 

INCLUDED:  3DXTECH High-Temp Filament Package.  The Funmat HT Printer comes with 5 rolls of our high-performance filament.  We add a 250g reel of CF-Ultem, Ultem 9085, Ultem 1010, PPSU, and PSU to your order.  These materials are perfect for you to get accustomed to your new printer and to start creating amazing things right from the start!

INTAMSYS Funmat HT
General Purpose Engineering Grades High-Performance
PLA Nylon PSU
ABS PC/ABS PPSU
ASA PC/ASA Ultem PEI
PETG PC PEEK
CarbonX™ Carbon Fiber Ultem, PC, Nylon, PETG, ABS, PLA
3DXSTAT™ ESD-Safe Ultem, PC, PETG, ABS

 

Key Features of the Funmat HT High-Temperature 3D Printer

  • Heated Environment: Fully enclosed actively heated build chamber and internal filament storage
  • All Metal High-Temp Hot End:  Capable of reaching 450°C
  • Large Heated Build Plate:  10" x 10" build plate capable of reaching 160°C

Technical Specifications

Manufacturer INTAMSYS
Build Volume 260mm x 260mm x 260mm  [10" x 10" x 10"]
Product Dimensions 540mm x 500mm x 650mm
Product Weight 45kg
Build Platform Aluminum Plate + Borosilicate Glass
Layer Thickness (Typical) 0.05mm-0.3mm
Number of Extruders One
Nozzle Diameter 0.4mm
Nozzle Construction Stainless Steel (A2 Hardened Available)
Print Speed 30-300mm/s
Travel Speed 150mm/s
Supported File Types STL
Supported Filaments (Open Source) PEEK, ULTEM PEI, PPSU, PSU, PC, PC/ABS, Nylon, Carbon Fiber, ESD-Safe, PETG, ASA, ABS, PLA
Filament Diameter 1.75mm
Chamber Temperature Up to 90°C
Extruder Temperature Up to 450°C
Build Plate Temperature Up to 160°C
Operating Ambient Temperature Up to 35°C
Position Accuracy X/Y 12.5μm, Z 1.25μm
Build Plate Leveling Manual
Feeder Type Geared Feeder
Connectivity SD card, USB
Input 100~120V,18A/200~240V,10.5A,50~60Hz,1200W
Output DC 24V, 25A
Operating Sound 55-59db
Supported OS Windows/Linux/Mac OS
Software I-Suit (Cura based), Compatible with Simplify3D
Warranty 12 Month Limited (excl. Extruder )

 