10Kg Reel of MAX-G™ PETG Filament, Jet Black

XL sized 10Kg reel of MAX-G™ PETG is made using only premium resins and colorants.  We recommend this filament for use in practically any desktop 3D Printer that has a heated bed.

Benefits of MAX-G™ PETG include:

  • Brilliant Colors = Beautiful Parts!
  • Superior Chemical Resistance vs. ABS
  • BPA Free, FDA Compliant
  • Amorphous:  Low and near isotropic shrinkage
  • Low moisture absorption:  3X lower vs. ABS
  • Very low odor emitted during printing

10Kg Reel Dimensions:

  • Diameter:  16 inches
  • Width:  7.5 inches
  • Arbor Hole:  1.5 inches

Recommended Print Conditions:

  • Extruder:  Ideally 230 to 260°C
  • Platform Temp:  60 to 90°C
  • Platform Prep:  Clean glass w/ Kapton Tape, PVA-based glue, or hairspray
  • Support:  Our Aquatek water soluble support works great to create complex parts.  This support can be found HERE.  
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.