Glow in the dark PETG

MAX-G™ PETG 3D Filament, Glow In The Dark, 750g


MAX-G™ PETG Filament, Glow in the Dark

MAX-G™ PETG is made using only premium resins and colorants.  Our glow in the dark will PETG is an awesome addition to the fun prints you make for work, family, and friends.  Charge this up in bright light (LED lights are the best) and the material glows a bright green.  

Benefits of MAX-G™ PETG include:

  • Brilliant Colors = Beautiful Parts!
  • Superior Chemical Resistance vs. ABS
  • BPA Free, FDA Compliant
  • Amorphous:  Low and near isotropic shrinkage
  • Low moisture absorption:  3X lower vs. ABS
  • Very low odor emitted during printing

Recommended Print Conditions:

  • Extruder:  Ideally 230 to 260°C
  • Platform Temp:  60 to 90°C
  • Platform Prep:  Clean glass w/ Kapton Tape or Hairspray