5-Pack PETG 3D Printing Filament

MAX-G™ PETG, 4kg Reels, 5-Pack Special Order

$495.00
Lead Time:
2 to 3 weeks

4KG XL Reels of PETG 3D Printing Filament 5-Pack [Special Order]

MAX-G™ PETG is made using only premium resins and colorants.  We recommend this filament for use in practically any desktop 3D Printer that has a heated bed.  Our filament is precision extruded onto 4kg reels (8.8 lbs) and then vacuum-sealed with desiccant to protect it from moisture. 

Please note:

  • This product is made to order, please allow up to 2 to 3 weeks lead time for your order to be produced and ready to ship
  • All other products in your order will ship with the 5-pack (no partial shipments)
  • One color only in 5-packs (no mixing of colors)

Reel Specs:

  • 12" diameter, 4" traverse, 2" arbor hole

Filament diameter specs:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  230-260°C
  • Bed Temp:  60-90°C 
  • Bed Prep:  Clean glass w/ Kapton Tape, PVA-based glue, or hairspray
  • Support:  Our Aquatek water soluble support works great to create complex parts.  This support can be found HERE.  
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.