Copper ABS Filament

Metallic Copper ABS, 1kg

$29.95

Metallic Copper ABS 3D Printing Filament, 1kg Reel

3DXTech™ ABS is made in the USA using 100% virgin resin and colorants - precision extruded onto 1kg reels (2.2 lbs.).  The filament is then vacuum-sealed with desiccant to protect it from moisture.  

For use with desktop printers such as Makerbot, Reprap, Printrbot jr., Makerfarm Prusa i3, MendelMax, UP! 3D, Flashforge, Solidoodle,
Afinia, Lulzbot Taz3/4, Makergear, Ultimaker, or any other printer accepting 1.75mm or 3.0mm filament.  

Filament diameter specs:  

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

1-3d-filament-technical-data.png

Recommended Print Conditions:

  • Extruder Temp:  220-240°C, Ideal 230°C
  • Bed Temp:  100-110°C
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry