Geloy PC/ASA for home extrusion

PC/ASA Pellets

$20.00

Geloy® PC/ASA Pellets (Bright White)

Our premium Sabic Geloy® UV-stable & weatherable PC-ASA resin is ideal for home extrusion enthusiasts.  Make your own high-performance Geloy® PC/ASA filament with a home-extruder.  Available in bright white only.

Processing Recommendations:

  • Pre-dry before extrusion at 110°C for 4 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  230 - 250°C