MAX-G™ PETG Filament, Jet Black
MAX-G™ PETG is made using only premium resins and colorants. Our PETG is a durable material that has excellent Z-layer strength while remaining flexible. The base resin used in our PETG filament is FDA approved and has improved chemical resistance compared to PLA or ABS - and it is suitable for cleaning with isopropyl alcohol as needed.
Benefits of MAX-G™ PETG include:
- Superior Chemical Resistance vs. ABS and PLA
- BPA Free, FDA Compliant
- Amorphous: Low and near isotropic shrinkage
- Low moisture absorption: 3X lower vs. ABS
- Very low odor emitted during printing
4kg Reel Dimensions: 12" diameter, 3.5" wide, 2" center hole
Recommended Print Conditions:
- Extruder: Ideally 230 to 260°C
- Platform Temp: 60 to 90°C
- Platform Prep: Clean glass w/ Kapton Tape, PVA-based glue, or hairspray
- Support: Our Aquatek water soluble support works great to create complex parts. This support can be found HERE.
- Drying Instructions: Please see the following instructions for when you want to dry out this filament, HERE.