ECOMAX® PLA Biopolymer is made in the USA using 100% virgin PLA Naturworks biopolymer resin and premium colorants.  Our filament is precision extruded onto 1kg reels (2.2 lbs) and then vacuum-sealed with desiccant to protect it from moisture.  

This filament is ideal for use with practically all desktop printers, such as Makerbot, Prusa, Ender, Flashforge, Anet, Creality, Lulzbot, Makergear, Ultimaker, or any other printer accepting 1.75mm or 2.85mm filament.

Check out AquaTek X1 Water Soluble Support (HERE).  Works great with PLA and a wide array of materials.  

The "closest" Pantone matches for our PLA colors are:

  • Red: Pantone 1795C 
  • True Red:  Pantone 200C
  • Blue: Pantone 2152C
  • Green: Pantone 348C
  • Yellow: Pantone 121C
  • Orange: Pantone 1485C
  • Cool Grey: Pantone 8C
  • Dark Grey:  Pantone 10C
Filament diameter specs:
  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  190-220°C
  • Bed Temp:  23-60°C [No Heated Bed Required]