Ideal for making your own filament or for use in a pellet fed 3D printer.  

Processing Recommendations:

  • Pre-dry before extrusion at 80°C for 2-4 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  190 - 210°C 