Make your own high-performance BVOH support filament or use as support material with pellet fed printers.  

Processing Recommendations:

  • Pre-dry before extrusion at 50°C for 4-6 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  150 - 170°C depending on your extruder set-up.
  • Do not cool using water tanks - this is a water soluble material and will dissolve in the water.
  • BVOH filament is relatively brittle and filament made using this polymer may be difficult to handle without breaking.