3DXMAX® ASA
3DXMAX® ASA (Acrylonitirle Styrene Acrylate) is a UV-resistant, famously weatherable polymer. Our ASA has a low-gloss matte finish which makes it the perfect filament for technical-looking prints, especially when you don’t want the high-gloss surface finish often associated with 3D printing materials like ABS, PETG, or PLA.
Gearbox HT2™ 3D Printer:
Print industrial-grade parts using our ASA and more with the new Gearbox™ HT2 High-Temp 3D Printer.

Extruder Temp
235-255°C

Bed Temp
90-110°C

Heated Chamber
Recommended

Nozzle Specs
No special concerns

Bed Adhesion
Magigoo Bed Prep

Layer Height
No special concerns

Drying Specs
80°C for 4 hours

Supports
Works best with
X1 USM Water Soluble Support
Benefits of 3DXMAX® ASA:
- Excellent mechanical and thermal properties (Tg of 105°C)
- Highly resistant to ultra-violet radiation and sunlight
- Sturdy and rugged against the weather, ideal for an outdoor part
- Easier to print than most industrial-grade materials
- Variety of colors and beautiful, low-gloss finish to make your models pop!
ASA is the Material for Outdoor Use:
ASA’s UV-stability makes it an ideal material for outdoor applications which experience intense exposure to the sun and elements. ASA’s exceptional mechanical and thermal properties – coupled with excellent UV-stability – is why this resin is used in the Auto, Marine, and RV industries.
Typical ASA Applications Include:
Mirror Housings, Cowl Covers, Radiator Grills, & Sensor Housings

Filament Specifications:
1.75mm and 2.85mm +/- 0.05mm in diameter
Recommended Print Settings:
- Extruder: 235-255°C
- Bed Temp: 90-110°C
- Other: Lower the bed temp down by about 10-20°C after the first few layers. The use of a fan at up to 50% may be needed for printers without enclosed and heated chambers.
- Bed Prep: Magigoo Bed Prep Adhesive and 3DXTECH Polyimide Tape work best for us.
- Heated Chamber: Recommended, a chamber helps reduce warping.
- Supports: Water soluble AquaTek X1 USM works great for complex parts.
- Drying Instructions: 80°C for 4 hours.