3DXMAX® ASA

3DXMAX® ASA (Acrylonitirle Styrene Acrylate) is a UV-resistant, famously weatherable polymer. Our ASA has a low-gloss matte finish which makes it the perfect filament for technical-looking prints, especially when you don’t want the high-gloss surface finish often associated with 3D printing materials like ABS, PETG, or PLA.

Ext Temp 1

Extruder Temp
235-255°C

Bed Temp

Bed Temp
90-110°C

Chamber Temp

Heated Chamber
Recommended

Nozzle Settings

Nozzle Specs
No special concerns

Bed Adhesion

Bed Adhesion
Magigoo Bed Prep

Layer Height

Layer Height
No special concerns

Drying Filamen

Drying Specs
80°C for 4 hours

Water Soluble Support

Supports
Works best with
X1 USM Water Soluble Support

Benefits of 3DXMAX® ASA:

  • Excellent mechanical and thermal properties (Tg of 105°C)
  • Highly resistant to ultra-violet radiation and sunlight
  • Sturdy and rugged against the weather, ideal for an outdoor part
  • Easier to print than most industrial-grade materials
  • Variety of colors and beautiful, low-gloss finish to make your models pop!

ASA is the Material for Outdoor Use:

ASA’s UV-stability makes it an ideal material for outdoor applications which experience intense exposure to the sun and elements. ASA’s exceptional mechanical and thermal properties – coupled with excellent UV-stability – is why this resin is used in the Auto, Marine, and RV industries.

Typical ASA Applications Include:

Mirror Housings, Cowl Covers, Radiator Grills, & Sensor Housings

asa bird feeder

Filament Specifications:

1.75mm and 2.85mm +/- 0.05mm in diameter

Recommended Print Settings:

  • Extruder: 235-255°C
  • Bed Temp: 90-110°C
  • Other: Lower the bed temp down by about 10-20°C after the first few layers
  • Bed Prep: Magigoo Bed Prep Adhesive and 3DXTECH Polyimide Tape work best for us.
  • Heated Chamber: Recommended, a chamber helps reduce warping.
  • Supports: Water soluble AquaTek X1 USM works great for complex parts.
  • Drying Instructions: 80°C for 4 hours.