3DXTECH Filaments
Open Source 3D printing filament for all desktop printers. Try Carbon Fiber, ESD-Safe, and Glass Fiber materials manufactured in the United States by 3DXTECH.
3DXTECH Filaments
$16.00 – $42.00
3DXMAX® ASA is an excellent choice for printing production or prototype parts. This material is more durable than ABS, has lower gloss, and has the added benefit of being UV-stable for exterior applications.
3DXMAX® ASA (Acrylonitirle Styrene Acrylate) is a UV-resistant, famously weatherable polymer. Our ASA has a low-gloss matte finish which makes it the perfect filament for technical-looking prints, especially when you don’t want the high-gloss surface finish often associated with 3D printing materials like ABS, PETG, or PLA.
Print industrial-grade parts using our ASA and more with the new Gearbox™ HT2 High-Temp 3D Printer.
Extruder Temp
235-255°C
Bed Temp
90-110°C
Heated Chamber
Recommended
Nozzle Specs
No special concerns
Bed Adhesion
Magigoo Bed Prep
Layer Height
No special concerns
Drying Specs
80°C for 4 hours
Supports
Works best with
X1 USM Water Soluble Support
ASA’s UV-stability makes it an ideal material for outdoor applications which experience intense exposure to the sun and elements. ASA’s exceptional mechanical and thermal properties – coupled with excellent UV-stability – is why this resin is used in the Auto, Marine, and RV industries.
Mirror Housings, Cowl Covers, Radiator Grills, & Sensor Housings
1.75mm and 2.85mm +/- 0.05mm in diameter