3DXMAX® PC/ASA

3DXMAX® PC/ASA (Polycarbonate + Acrylonitirle Styrene Acrylate Alloy) is a highly UV-resistant weatherable polymer.   PC/ASA’s UV-stability makes it an ideal material for outdoor applications that will experience intense exposure to the sun and weather.  PC/ASA’s exceptional mechanical and thermal properties – coupled with excellent UV-stability – is why this resin is used the Auto, Marine, and RV industries for exterior applications such as mirror housings, cowl covers, radiator grills, and sensor housings.
Note: This product is discontinued.

Diameter Specifications:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  270 – 290°C
  • Bed Temp:  110 – 120°C, cool the bed down by about 10-20°C after the first couple of layers
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry, or Hairspray on clean glass
  • Enclosure:   We recommend using a printer with an enclosure to help keep some heat in while printing with PC/ASA
  • Support:  Our Aquatek water soluble support works great to create complex parts.  This support can be found HERE.
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.