3DXSTAT ESD-PLA
3DXSTAT ESD-PLA

3DXSTAT ESD-PLA

SKU: PLA02ES100750BK00

Regular price
$98.00
Sale price
$98.00
Regular price
$0.00
Color Code: Black
Diameter:
Reel Size:
In Stock
Description
3DXSTAT ESD PLA is an advanced ESD-Safe compound designed for use in critical applications which require electrostatic discharge (ESD) protection. Made using cutting-edge multi-wall carbon nanotube technology, state of the art compounding technology, and precision extrusion processes. Target surface resistance: 10⁴-10⁹ Ohm.

Benefits of 3DXSTAT ESD-PLA

  • Ideal for printing without a heated bed, no enclosure required
  • Low shrinkage, warping, and easy printability, PLA prints on practically all desktop 3D printers
  • Very low odor, perfect for printing in home or office environments
  • Gorgeous surface quality to make printed parts look beautiful
  • Made from plants makes PLA a renewable biopolymer
Reviews

Print Recommendations

365-390°C
Extruder Temp
210-240C
140-160°C
Bed Temp
23-60C
Recommended
Heated Chamber
Not required
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
65C for 4 hours
Nozzle-Abrasion

Abrasive Material

This material is particularly abrasive among 3D printing filaments. Users may find standard brass nozzles are chewed through very quickly compared to standard wear and tear. When worn through, the nozzle diameter will widen inconsistently and the printer will experience extrusion issues.

Because of this, it's strongly recommended this material be printed through a hardened steel nozzle rather than a softer metal. Hardened steel nozzles can often be inexpensive and easily installed depending on your printer manufacturer's instructions.

Material DETAILS

Glass Fiber Reinforced Filament

Rectangle111

What Is It?

DescriptionFibers made of glass reinforced into the polymer during manufacturing and aligned along the axis of filament. This, along with their physical makeup, give this material enormous strength and mechanical properties.
Rectangle222

What Does It Do?

Glass fiber reinforcement gives material a lot of desirable properties: High strength High stiffness High chemical resistance Low thermal expansion
Rectangle333

How Does It Work?

Reinforcing plastic with glass fibers produces a 3D printing filament which exhibits the best properties of both fiberglass and the plastic of choice.
Rectangle444

What Is It Good For?

Ideal for any applications which require strength and rigidity. For these reasons, glass fiber reinforced filament is very popular in automotive, mechanical, civil engineering, and research industries.
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.