3DXTECH™ ABS 4kg XL Reels 3D Printing Filament
3DXTECH™ ABS 4kg is made in the USA using 100% virgin resin and colorants – precision extruded onto 4kg reels (8.8 lbs.). The filament is then vacuum-sealed with desiccant to protect it from moisture.
Print industrial-grade ABS 4kg parts with Gearbox™ HT2 High-Temp 3D Printer. Check it out HERE.
For use with practically ANY desktop printer that can print with ABS (heated print bed), including Airwolf, Ultimaker, Makerbot, Reprap, Prusa i3, MendelMax, UP! 3D, Flashforge, Solidoodle, Afinia, Lulzbot Taz (all models), Makergear…
- 12″ diameter, 4″ traverse, 2″ arbor hole
Filament diameter specs:
- 1.75mm +/- 0.05mm
- 2.85mm +/- 0.05mm
Recommended Print Conditions: