AquaTek™ BVOH [Butendiol Vinyl Alcohol] water soluble support is our original support material created for printing complex parts. BVOH offers good adhesion to a wide variety of model materials and is warm water soluble for easy support removal.
Our BVOH Water Soluble Support is an advanced water-soluble support filament based on a specialty copolymer of Butendiol Vinyl Alcohol. This filament is ideal for printing complex parts using PLA, ABS, ASA, PETG.
AquaTek™ BVOH is completely soluble in warm water and is easily removed from the printed part.
Extruder Temp
190-220°C
Bed Temp
23-90°C
Heated Chamber
Not required
Nozzle Specs
No special concerns
Bed Adhesion
Magigoo Bed Prep Adhesives
Nano Polymer Adhesive
Layer Height
No special concerns
Drying Specs
65°C for 2-4 hours
Supports
BVOH is water soluble
This material doesn’t yet have a formal TDS.
1.75mm and 2.85mm +/- 0.05mm in diameter