CarbonX™ PC-ABS+CF is made using a low-gloss PC-ABS and reinforced with premium high-modulus carbon fiber. This material offers ease of printing, high thermal properties, strength & stiffness, excellent dimensional stability, and an amazing low-gloss surface finish.
CarbonX™ PC-ABS+CF has been formulated to offer improved thermal resistance and mechanical properties while retaining an ease of printability that makes it ideal for anyone seeking a structural component with high heat, high stiffness, excellent surface quality, and dimensional stability.
Print industrial-grade Carbon Fiber PC/ABS parts with Gearbox™ HT2 High-Temp 3D Printer.
Our AquaTek® water soluble X1 Universal Support Material works great with CarbonX™ PC-ABS+CF and allows you to print parts with complex geometries and then dissolve away the support in warm water.
Recommended Print Conditions: