FibreX™ TPU+GF30 Thermoplastic Polyurethane 3D Printer Filament
FibreX™ TPU+GF30 elastomer is an engineering-grade material that we chose based on its balance of printability, flexibility, chemical resistance, and toughness. 3DXFLEX™ TPU+GF30 has a hardness of 60D, allowing you to make very tough, impact resistant, flexible prints. We recommend direct-drive extruders, but experienced users can be successful with Bowden-type drives as well.
Print Recommendations

Extruder Temp
230-255°C

Bed Temp
23°-50°C

Heated Chamber
Not required

Nozzle Specs
0.4mm diameter minimum
Hardened Steel Nozzle

Bed Adhesion
Magigoo Bed Prep

Layer Height
0.25mm or higher

Drying Specs
65°C for 4 hours

Supports
Water Soluble Support
Benefits of FibreX™ TPU+GF30 (60D) Include:
- Shore 60D semi-flex hardness
- Ease of printing compared to similar flexible materials
- Excellent layer bonding
- Outstanding fatigue resistance
- Very low odor emitted while printing
- Low moisture absorption
- Retains flexibility even at low temperature
- Styrene and BPA free
Filament Specifications:
1.75mm and 2.85mm +/- 0.05mm in diameter
Recommended Print Settings:
- Extruder: 230-255°C
- Bed Temp: 23-40°C
- Bed Prep: Magigoo Bed Prep or 3DXTECH Polyimide Tape gives us the best results
- Heated Chamber: Not required
- Supports: AquaTek™ water soluble X1 USM Universal Support Material works ideal for complex parts
- Drying Instructions: 65°C for 4 hours