FluorX PVDF

$75.00$250.00

4 interest-free payments with Klarna-Logo-Icon  Learn More

FluorX™ PVDF [Polyvinylidene Fluoride] is made using Arkema Kynar®. PVDF is an excellent choice for applications that require chemical resistance, high-heat resistance, and superior abrasion resistance.

SKU: Select options above Brand: FluorX™ Categories: ,

FluorX™ PVDF 3D Filament

PVDF [Polyvinylidene fluoride] is a high-performance polymer which offers exceptional thermal and chemical resistances.

Rated for uses up to 130°C – this filament can be used in demanding applications under the most extreme conditions. PVDF is resistant to most chemicals and solvents, making it a great fit for applications which will be exposed to harsh environments.

Ext Temp 1

Extruder Temp
245-265°C

Bed Temp

Bed Temp
90-110°C

Chamber Temp

Heated Chamber
Not required

Nozzle Settings

Nozzle Specs
No special concerns

Bed Adhesion

Bed Adhesion
Nano Polymer Adhesive

Layer Height

Layer Height
No special concerns

Drying Filamen

Drying Specs
Not required

Break Away Support

Supports
Works great with break-away support

Benefits of PVDF Include:

  • High Thermal Properties: 130°C CUT
  • Excellent resistance to a broad range of chemicals, such as automotive fluids, oils, gas, lubricants, fully halogenated hydrocarbons, alcohols, acids, and bases
  • Non-hygroscopic, does not absorb moisture. No drying needed!
  • Inherently UV-resistant with very stable H-F bonds.
  • Low smoke and flame characteristics with a base resin rated V-0
  • Long-term hydrolytic stability
  • Resistant to nuclear radiation
  • Very good abrasion resistance – similar to Nylon and UHMW-PE for high-wear applications

Filament Specifications:

1.75mm and 2.85mm +/- 0.05mm in diameter

Recommended Print Settings:

  • Extruder: Between 245 and 265°C depending on your printer. Some need to get as high as 280°C.
  • Platform Temp: 90 – 110°C
  • Bed Prep: Nano Polymer Adhesive gives us the best results.
  • Other: No or slow cooling fan. Print with speeds of 40-60mm/s as a good starting point.
  • Drying Instructions: PVDF doesn’t absorb moisture, and doesn’t need drying!
  • Safety note: This polymer starts to degrade and break down at temps above 290°C. Please keep your extruder temperature below that point to avoid degradation, offgassing, and mechanical property loss.