GF30 Nylon 6 Pellets

$120.00$665.00

4 interest-free payments with Klarna-Logo-Icon  Learn More

GF30 PA6 Pellets are ideal for Filastruder, Filabot, and Noztek type home extruders.
Contact us for larger quantities.

SKU: Select options above Category:

GF30 PA6 Pellets [30% Glass Fiber Nylon 6]

Ideal for home extrusion enthusiasts.  Make your own GF-Nylon filament with a home-extruder such as the Filabot and Filastruder or others that are set-up for high-temp extrusion.

Processing Recommendations:

  • Pre-dry before extrusion at 90°C for 4-6 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  220-240°C (depending upon how your heater bands, thermocouple, and PID are configured.)