3DXMAX LTS1 Low-Temp Support Filament [ABS Break Away Support]
![3DXMAX LTS1 Low-Temp Support [ABS BAS] Ext Temp 1 Ext Temp 1](https://www.3dxtech.com/wp-content/uploads/2021/01/Ext-Temp-1-1024x1024.jpg)
Extruder Temp
220-235°C
![3DXMAX LTS1 Low-Temp Support [ABS BAS] Bed Temp Bed Temp](https://www.3dxtech.com/wp-content/uploads/2021/01/Bed-Temp-1024x1024.jpg)
Bed Temp
100-110°C
![3DXMAX LTS1 Low-Temp Support [ABS BAS] Chamber Temp Chamber Temp](https://www.3dxtech.com/wp-content/uploads/2021/01/Chamber-Temp-1024x1024.jpg)
Heated Chamber
Not required
![3DXMAX LTS1 Low-Temp Support [ABS BAS] Nozzle Settings Nozzle Settings](https://www.3dxtech.com/wp-content/uploads/2021/01/Nozzle-Settings-1024x1024.jpg)
Nozzle Specs
No special concerns
Benefits of 3DXMAX™ LTS1:
- Bullet Points for LTS1
- Additional bullet points
![3DXMAX LTS1 Low-Temp Support [ABS BAS] iconfinder 1 02 511559 Technical Data Sheet](/wp-content/uploads/2020/11/iconfinder_1-02_511559-300x300.png)
Technical Data Sheet
This material doesn’t yet have a formal TDS.
![3DXMAX LTS1 Low-Temp Support [ABS BAS] iconfinder 1 02 511559 Safety Data Sheet](/wp-content/uploads/2020/11/iconfinder_1-02_511559-300x300.png)
Safety Data Sheet
This material doesn’t yet have a formal SDS.
Filament Specifications:
1.75mm and 2.85mm +/- 0.05mm in diameter
Recommended Print Settings:
- Extruder: 220-235°C
- Bed Temp: 100-110°C
- Bed Prep: Magigoo Bed Prep gives us the best results.
- Heated Chamber: Not required
- Drying Instructions: No drying needed at all!