PEI 9085 Pellets [Ultem™ 9085]

$365.00$2,155.00

4 interest-free payments with Klarna-Logo-Icon  Learn More

Ultem PEI 9085 Pellets are ideal for Filastruder, Filabot, and Noztek type home extruders.
Contact us for larger quantities.

SKU: Select options above Category:

PEI 9085 Pellets – Natural

PEI 9085 Pellets are ideal for home extrusion enthusiasts.  Make your own PEI 9085 filament with a home-extruder such as the Filabot and Filastruder or others that are set-up for high-temp extrusion.

Processing Recommendations:

  • Pre-dry before extrusion at 150°C for 4-6 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  330 – 350°C (depending upon how your heater bands, thermocouple, and PID are configured.)

Questions?