Extrude your own 3D filament using our PVA resin for extruders such as Filabot, Filastruder, and Noztek

SKU: Select options above Category:

PVA Water Soluble Support Pellets

Ideal for making your own filament or for use in a pellet-fed 3D printer.

Please note:  Additional shipping charges may apply on orders over 10kg.

Processing Recommendations:

  • Pre-dry before extrusion at 50°C for 4-6 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  150 – 170°C depending on your extruder set-up.
  • Do not cool using water tanks – this is a water soluble material and will dissolve in the water.

Questions?

Send us a message and we'll reach out as soon as we can!