ThermaX HTS2 High-Temp [9085 BAS]

$125.00$450.00

ThermaX™ HTS2 [High Temperature Support] break away support is ideal for printing high-temperature polymers including PSU, PES, PPSU, PPS, Ultem™ PEI, PEKK, and PEEK. This support adheres well to these advanced materials and then is broken away after printing to allow for complex geometry without damaging your part.

SKU: Select options above Brand: ThermaX™ Categories: ,

Thermax™ HTS2 High-Temp Support Filament [9085 Break Away Support]

Our break away high-temp support filament is ideal for use in dual extruder 3D printers designed to print high-temp materials.

HTS is the premium support for our high-temp products, unlike most support filaments, which are not designed to withstand the heat required to print the top-end of performance materials.

Gearbox HT2™ 3D Printer: Print industrial-grade parts using our HTS Filament and more with the new Gearbox™ HT2 High-Temp 3D Printer.

Print Recommendations

Ext Temp 1

Extruder Temp
350-380°C

Bed Temp

Bed Temp
120-160°C

Chamber Temp

Heated Chamber
Recommended
(No higher than 185°C)

Nozzle Settings

Nozzle Specs
No special concerns

Bed Adhesion

Bed Adhesion
Nano Polymer Adhesive

Layer Height

Layer Height
No special concerns

Drying Filamen

Drying Specs
120°C for 4 hours

Break Away Support

Supports
HTS is break-away

Support Removal:

  • This is break-away support and does not dissolve.
  • High-Temp support is best removed while printed part is still warm.
  • If the finished printed part cools completely and the support removal gets too difficult, you can re-warm the part in the printer chamber or an oven not exceeding the Tg of the model material you are printing with.

Filament Specifications:

1.75mm and 2.85mm +/- 0.05mm in diameter

Recommended Print Settings:

  • Extruder: 350-380°C
  • Bed Temp: 120-160°C
  • Bed Prep: Nano Polymer Adhesive or Polyimide Tape gives us the best results.
  • Heated Chamber: All high-temp materials print better with a heated enclosure or build environment. Enclosure temp should not exceed 185°C for our high-temp support material to remain structurally sound as a support.
  • Other: Don’t use a cooling fan while printing this support.
  • Drying Instructions: 120°C for 4 hours

ULTEM™ is a registered trademark of Sabic Innovative Plastics.