{"product_id":"3dxflex-peba-90a","title":"3DXFLEX™ PEBA (90A)","description":"\u003cdiv class=\"pdp-description-row\"\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\n\u003ch2\u003e3DXFLEX™ PEBA (90A)\u003c\/h2\u003e\n\u003cp\u003eUnlike TPUs of equivalent durometer, PEBA 90A has a lower density and higher energy rebound, perfect for applications requiring lightweight parts which can withstand significant impacts. PEBA 90A also retains its impressive impact resistance at low temperatures, ensuring consistent performance in challenging environments. Able to be printed with a nozzle temperature below 250°C, PEBA 90A is an engineering-grade material that doesn’t require industrial equipment to print.\u003c\/p\u003e\n\u003ch5\u003eMADE IN THE USA\u003c\/h5\u003e\n\u003cp\u003eWe manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.\u003c\/p\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\u003cimg src=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/3DXFLEXPEBABlack-2webtransparent.png?v=1793915187\"\u003e\u003c\/div\u003e\n\u003c\/div\u003e","brand":"3DXTECH","offers":[{"title":"Black \/ 1.75mm \/ 750g","offer_id":53136369582443,"sku":"163BK06A-750G","price":140.0,"currency_code":"USD","in_stock":false},{"title":"Natural \/ 1.75mm \/ 750g","offer_id":53136369615211,"sku":"163NT00A-750G","price":140.0,"currency_code":"USD","in_stock":false}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/3DXFLEXPEBABlackwebtransparent.png?v=1793915187","url":"https:\/\/www.3dxtech.com\/products\/3dxflex-peba-90a","provider":"3DXTECH","version":"1.0","type":"link"}