{"product_id":"3dxlabs™-emi-abs-black-1-75mm-750g","title":"3DXLABS™ EMI-ABS, Black, 1.75mm, 750g","description":"\u003cdiv class=\"pdp-description-row\"\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\n\u003ch2\u003e3DXLABS™ EMI-ABS\u003c\/h2\u003e\n\u003ch5\u003e**3DXLABS R\u0026amp;D PRODUCT**\u003c\/h5\u003e\n\u003cp\u003eBe among the first to test our latest development: EMI-ABS, a cutting-edge, electrically conductive ABS blend engineered to provide EMI shielding performance in FDM 3D printing applications.\u003c\/p\u003e\n\u003cp\u003eAs part of our 3DXLabs R\u0026amp;D program, this material is available exclusively to our experienced users who want early access to experimental formulations and the opportunity to shape future products through direct feedback.\u003c\/p\u003e\n\u003cp data-start=\"606\" data-end=\"623\"\u003e\u003cstrong data-start=\"606\" data-end=\"622\"\u003eKey Features\u003c\/strong\u003e:\u003c\/p\u003e\n\u003cul data-start=\"624\" data-end=\"1188\"\u003e\n\u003cli data-start=\"624\" data-end=\"917\"\u003e\n\u003cp data-start=\"626\" data-end=\"658\"\u003e\u003cstrong data-start=\"626\" data-end=\"655\"\u003eEMI Shielding Performance\u003c\/strong\u003e:\u003c\/p\u003e\n\u003cul data-start=\"661\" data-end=\"917\"\u003e\n\u003cli data-start=\"661\" data-end=\"719\"\u003e\n\u003cp data-start=\"663\" data-end=\"719\"\u003eNear \u003cstrong data-start=\"668\" data-end=\"676\"\u003e0 dB\u003c\/strong\u003e shielding effectiveness below \u003cstrong data-start=\"707\" data-end=\"717\"\u003e500MHz\u003c\/strong\u003e\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli data-start=\"722\" data-end=\"799\"\u003e\n\u003cp data-start=\"724\" data-end=\"799\"\u003eBegins increasing at \u003cstrong data-start=\"745\" data-end=\"755\"\u003e600MHz\u003c\/strong\u003e, with strong performance above \u003cstrong data-start=\"787\" data-end=\"797\"\u003e700MHz\u003c\/strong\u003e\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli data-start=\"802\" data-end=\"917\"\u003e\n\u003cp data-start=\"804\" data-end=\"917\"\u003eBetween \u003cstrong data-start=\"812\" data-end=\"830\"\u003e4 dB and 16 dB\u003c\/strong\u003e shielding effectiveness from \u003cstrong data-start=\"860\" data-end=\"876\"\u003e1GHz to 9GHz\u003c\/strong\u003e, depending on infill pattern and density\u003c\/p\u003e\n\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003c\/li\u003e\n\u003cli data-start=\"919\" data-end=\"1188\"\u003e\n\u003cp data-start=\"921\" data-end=\"940\"\u003e\u003cstrong data-start=\"921\" data-end=\"937\"\u003ePrintability\u003c\/strong\u003e:\u003c\/p\u003e\n\u003cul data-start=\"943\" data-end=\"1188\"\u003e\n\u003cli data-start=\"943\" data-end=\"1050\"\u003e\n\u003cp data-start=\"945\" data-end=\"1050\"\u003eExcellent layer adhesion and surface quality when printed on \u003cstrong data-start=\"1006\" data-end=\"1019\"\u003eBambu X1C\u003c\/strong\u003e (no heated chamber required)\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli data-start=\"1053\" data-end=\"1130\"\u003e\n\u003cp data-start=\"1055\" data-end=\"1130\"\u003e\u003cstrong data-start=\"1055\" data-end=\"1085\"\u003eHeated chamber recommended\u003c\/strong\u003e to maximize mechanical strength and finish\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli data-start=\"1133\" data-end=\"1188\"\u003e\n\u003cp data-start=\"1135\" data-end=\"1188\"\u003e\u003cstrong data-start=\"1135\" data-end=\"1154\"\u003eMinimal warping\u003c\/strong\u003e compared to standard unfilled ABS\u003c\/p\u003e\n\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003c\/li\u003e\n\u003cli data-start=\"919\" data-end=\"1188\"\u003e\n\u003cp data-start=\"921\" data-end=\"940\"\u003e\u003cstrong data-start=\"921\" data-end=\"937\"\u003eRecommended Print Settings\u003c\/strong\u003e:\u003c\/p\u003e\n\u003cul data-start=\"943\" data-end=\"1188\"\u003e\n\u003cli data-start=\"943\" data-end=\"1050\"\u003e\n\u003cp data-start=\"945\" data-end=\"1050\"\u003eNozzle Temp: 285°C\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli data-start=\"943\" data-end=\"1050\"\u003e\n\u003cp data-start=\"945\" data-end=\"1050\"\u003eBed Temp: 100°C\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli data-start=\"943\" data-end=\"1050\"\u003e\n\u003cp data-start=\"945\" data-end=\"1050\"\u003eMin. Chamber Temp: 60°C\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli data-start=\"943\" data-end=\"1050\"\u003e\n\u003cp data-start=\"945\" data-end=\"1050\"\u003eSpeed: 100 mm\/s\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli data-start=\"943\" data-end=\"1050\"\u003e\n\u003cp data-start=\"945\" data-end=\"1050\"\u003eNozzle Diameter: 0.40mm, Hardened Steel\u003c\/p\u003e\n\u003c\/li\u003e\n\u003cli data-start=\"943\" data-end=\"1050\"\u003eMin. Layer Height: 0.20mm\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003c\/li\u003e\n\u003c\/ul\u003e\n\u003cp data-start=\"1190\" data-end=\"1413\"\u003e\u003ca href=\"https:\/\/www.3dxtech.com\/pages\/3dxlabs\"\u003e\u003cstrong data-start=\"1190\" data-end=\"1228\"\u003e3DXLabs materials are experimental\u003c\/strong\u003e\u003c\/a\u003e and offered in limited batches. If you’re a seasoned user who wants to be at the forefront of 3D printing innovation, this is your chance to try EMI-ABS and help shape its development.\u003c\/p\u003e\n\u003ch5\u003eMADE IN THE USA\u003c\/h5\u003e\n\u003cp\u003eWe manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.\u003c\/p\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\u003cimg src=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/EMI-ABS-SheildingEffectiveness-1.jpg?v=1753453822\"\u003e\u003c\/div\u003e\n\u003c\/div\u003e","brand":"3DXTECH","offers":[{"title":"Default Title","offer_id":53796385948011,"sku":"040BK00A-750G","price":125.0,"currency_code":"USD","in_stock":false}],"url":"https:\/\/www.3dxtech.com\/products\/3dxlabs%e2%84%a2-emi-abs-black-1-75mm-750g","provider":"3DXTECH","version":"1.0","type":"link"}